Magnetics: Difference between revisions
Jump to navigation
Jump to search
Adamcolton (talk | contribs) No edit summary |
Adamcolton (talk | contribs) No edit summary |
||
| Line 1: | Line 1: | ||
Magnetics covers transformers and inductors | Magnetics covers transformers and inductors | ||
https://coefs.uncc.edu/mnoras/files/2013/03/Transformer-and-Inductor-Design-Handbook_Chapter_2.pdf | |||
== Transformer == | == Transformer == | ||
| Line 9: | Line 11: | ||
== Materials == | == Materials == | ||
* Powdered Iron: | * Laminated Iron Alloyws: 1.5-2.0T 50Hz-1KHz | ||
* | * Powdered Iron: 0.6-0.8T 1KHz - 100KHz | ||
* Ferrites: 0.25-0.5T 20KHz - 20MHz | |||
Higher tesla is associated with higher core losses, but also higher saturation. | |||
[[Category:Electronics]] | [[Category:Electronics]] | ||
[[Category:Notes]] | [[Category:Notes]] | ||
Revision as of 16:40, 2 May 2018
Magnetics covers transformers and inductors
https://coefs.uncc.edu/mnoras/files/2013/03/Transformer-and-Inductor-Design-Handbook_Chapter_2.pdf
Transformer
These are just a pain to understand
Larger transformers increase hysteresis loss.
The correct frequency is critical. Ideally, the frequency should be as low as possible without saturating the transformer. Higher frequency increases hysteresis loss.
Materials
- Laminated Iron Alloyws: 1.5-2.0T 50Hz-1KHz
- Powdered Iron: 0.6-0.8T 1KHz - 100KHz
- Ferrites: 0.25-0.5T 20KHz - 20MHz
Higher tesla is associated with higher core losses, but also higher saturation.